Paint cracks when it can no longer move with the surface, usually because it has become brittle with age, was applied too thickly, or went on before the coat underneath was dry. Scrape and sand cracked paint back to a sound surface, prime and repaint; cracks that run through the plaster or wall itself need checking first.

For homeowners with cracked paint on walls, ceilings, trim or exterior boards.

Request a free quote
GDPD painter working on an interior wall
GDPD painter working on an interior wall

Part of our interior painting guide.

Types of paint cracking

Paint cracks and what they usually mean
TypeLooks likeUsual cause
Hairline crackingFine cracks in the top coat onlyPaint aged and brittle, or too little flexibility
Crazing or alligatoringA pattern like crocodile skinHard coat over a softer one, or recoating too soon
Mud crackingDeep, irregular cracks in thick areasPaint or filler applied too thick
Cracks along joinsStraight lines at plasterboard joins or trimMovement in the building or joint
Cracks through the wallCrack continues through plaster or masonryStructural movement or settlement

How to fix cracked paint

  1. Check for lead on older homes before scraping or sanding: see our lead paint guide.
  2. Scrape off loose and flaking paint.
  3. Sand to feather the edges, or remove the cracked layer entirely if crazing is widespread.
  4. Fill any gaps with a suitable filler; use a flexible sealant where trim meets walls.
  5. Prime bare areas.
  6. Repaint with thin, even coats, respecting the recoat time.

Preventing paint cracking

  • Prepare and prime properly so the paint bonds.
  • Apply coats at the thickness on the label; two thin coats beat one heavy one.
  • Wait for the recoat time before the next coat.
  • Use flexible acrylic paint on timber that moves with the seasons.
  • Avoid painting in extreme heat: see painting in hot weather.

When a crack is a bigger problem

If a crack keeps reopening after repair, runs diagonally from the corners of doors and windows, or goes right through plaster or brick, the building may be moving. Have it checked by a builder or engineer before painting. Fine cracks at plasterboard joins are often seasonal movement and can be filled with a flexible filler.

Cracking, peeling and blistering

Cracks often turn into peeling as water gets in. Compare paint peeling and blistering paint, and see preparing walls for painting for the full preparation sequence.

Cracking on exterior timber

Outside, cracking usually starts where paint has aged in the sun or where timber moves most, such as joins, sills and end grain. Once water gets into the cracks, peeling and rot follow. Repaint before cracks spread across the boards; our guide to when to repaint your house exterior explains the signs.

Your questions

Can I paint over cracked paint?

Not without preparation. Remove loose paint and sand smooth, or the cracks will show through and the new coat may fail.

Why is my new paint cracking as it dries?

It is usually applied too thickly, or over a coat that was not yet dry. Thin coats and correct recoat times prevent it.

Are cracks in walls structural?

Most fine cracks are not. Cracks that reopen, widen or run through the wall material should be checked by a builder.

Can paint crack in cold weather?

Paint applied below its minimum temperature may not form a proper film and can crack later. Follow the temperature range on the label.

Cracked paint you want fixed properly?

Send photos of the cracks, near and far. We will diagnose them and give you a free quote.

Request a free quote

About this guide

We are Gary Dyer Painters and Decorators, a trade-qualified Manawatū painting company, Master Painters members and certified Resene Eco-Decorators. We prepare and repaint homes and commercial interiors across Manawatū. This guide was last reviewed in November 2026. If anything here needs correcting, email gary@gdpd.nz.